How to Refine Gold with Urea Greenway Biotech, Inc.
Allow the gold to sit in the nitric acid for 30 to 45 minutes. Add 120 milliliters of hydrochloric acid for every ounce of gold in the container. For 5 ounces of gold, that would be 600 milliliters of HCL. The addition of hydrochloric acid turns the mixture brown and can result in fumes. As the chemicals react and heat up, the gold .