Gold Flotation Process Froth Flotation (Sulphide Oxide ...
In the Lab stage (Ore variability Bench scale tests) has evidenced problems with the natural occurrence of excessive frothing even without aeration or addition of frother. The condition for the flotation tests was: 25 g/t CuSO4 35 g/t PAX. 70 g/t Aero 208 and the optimum grind were p80 106 microns. The overall gold recovery was 90%.